The changes in the structure of the slab and the signals that appeared in selected loading cycles are summarized in Figure 6. The first significant crack was registered with DIC under the load P = 30 kN (before it was noticeable). Changes in the shape were observed in all registered signals. Especially, the amplitude of C4 (PZT sensor near the lower edge of the slab) decreased most significantly. However, after the load was relieved, the crack partially closed, which resulted in increasing the signal amplitude to the level from the beginning of the experiment, leaving changes only in the shape of the signal. 1e1e36bf2d